What was the initial goal in the first attempt to create transparent wood?
To create wood that was almost as clear as glass, but much stronger and shatterproof.
Or swipe the card
60 cards
What was the initial goal in the first attempt to create transparent wood?
To create wood that was almost as clear as glass, but much stronger and shatterproof.
What were some common problems encountered during the first attempt to make transparent wood?
The pieces cracked after a day or so when trying to make larger ones, smaller pieces warped, and all pieces yellowed and cracked after several months.
What type of wood was used as a starting material for the improved transparent wood method?
Balsa wood.
What thickness of balsa wood strips was initially used for the transparent wood experiment?
An eighth of an inch, which is about 3.2mm.
What was the initial size of the balsa wood squares cut for the experiment?
About two centimeters by two centimeters.
What was the first step after cutting the balsa wood pieces, according to the paper's method?
Drying them in an oven at 105 C for 24 hours to remove any moisture.
What two main chemical treatments were required for the wood after drying?
Removing lignin and bleaching them white.
What chemicals were used in the last attempt to remove lignin and bleach the wood?
A boiling solution of sodium sulfite and sodium hydroxide for lignin removal, followed by 30% hydrogen peroxide for bleaching.
What chemical was used in the new method to remove lignin and bleach the wood simultaneously?
Sodium chloride with an acetate buffer solution at a pH of 4.6.
Why was sodium chloride (sodium chlorite) preferred over concentrated hydrogen peroxide for bleaching in the new method?
Sodium chloride has little to no regulation and is easily bought online, unlike concentrated hydrogen peroxide (above 30%) which is controlled in Canada due to its use in explosives.
What is 'Miracle Mineral Supplement' (MMS) and why is its sale concerning?
MMS is often sold as an alternative medicine claiming to cure various diseases, but chemically it is similar to dilute bleach, with no evidence of benefits and potential to harm internal organs.
How was the 1 weight percent sodium chloride with acetate buffer solution prepared?
125 ml of water, 1.67g of sodium acetate, and 1.15 ml of acetic acid were combined. After dissolving, 1.3g of sodium chloride was added.
What chemical reaction occurs as the wood treating solution warms up, leading to lignin removal and bleaching?
Acetic acid reacts with sodium chloride, releasing chlorous acid, which quickly breaks down into chlorine dioxide.
What is the role of lignin in wood, and what happens when it is removed?
Lignin acts like a glue holding wood fibers together and is responsible for wood's natural yellow color. Removing it makes the wood more porous, opens space between fibers, and eliminates the yellow color.
What percentage of lignin content was aimed for after the chemical treatment according to the paper?
From 25% down to about 3%.
How long did the wood pieces sit in the chlorine dioxide solution until they appeared white?
About seven hours.
After chemical treatment, what was the first step to clean the wood pieces?
Dropping them into distilled water and leaving them overnight for chemicals to diffuse out.
What series of solvent washings were performed after the distilled water soak, and why?
100% ethanol, then a 50/50 mixture of ethanol and acetone, and finally pure acetone. The major reason is to get rid of the water.
How did the delignified wood pieces, before plastic infusion, differ in strength compared to the first attempt?
They were still pretty tough and felt similar to before the treatment, unlike the first attempt where they became super soft and bendy.
What was the final major step to make the delignified wood transparent?
Infusing them with plastic.
What type of plastic resin was used in the first attempt for infusion, and what were its drawbacks?
Epoxy resin, which was a two-part mixture with limited working time and a tendency to turn yellow, especially with UV exposure.
Why was epoxy resin considered a major problem for transparent wood intended as a glass replacement?
Windows are constantly exposed to UV light, and epoxy has a tendency to turn yellow, which would result in a "nasty yellow window."
What plastic material was chosen for the improved method, and what were its advantages?
Methyl methacrylate (MMA), which polymerizes into acrylic (Plexiglas) and does not have the same yellowing issue as epoxy. Its polymerization is also triggered by heating, allowing control over hardening time.
What is AIBN, and what is its role in the polymerization of methyl methacrylate?
AIBN is an initiator. When heated above 40 C, it breaks down and releases free radicals, which initiate the polymerization process of MMA.
What process was required for MMA before it could be added to the wood?
It had to be partially polymerized, creating some short chains to prevent it from vaporizing during the oven curing.
What were the conditions for the partial polymerization of MMA?
Reacting it for 15 minutes at 75 C.
How was the partial polymerization of MMA stopped after 15 minutes?
By dropping the flask into ice water to quickly drop the temperature.
What equipment was used to infuse the wood with pre-polymerized MMA, and why?
A vacuum chamber. Air was pulled out of the wood, and acetone and unpolymerized MMA were boiled off, allowing the MMA to rush into the wood when the vacuum was released.
What happened during the vacuum cycles as the vacuum was pulled stronger?
Air was pulled out of the wood, and then acetone as well as some unpolymerized MMA started boiling off.
After vacuum infusion, why didn't the wood immediately become transparent?
It was thought that it would only clear up when the MMA was fully polymerized.
What was done with the MMA-infused wood pieces before final polymerization?
They were sandwiched between two pieces of glass and wrapped in aluminum foil.
What were the conditions for the final polymerization of MMA in the oven?
In an oven preheated to 70 C for four hours.
What was the initial problem after the first attempt at final polymerization with MMA?
The MMA had apparently disappeared, and the wood looked the exact same, indicating a complete failure.
What was suspected to be the cause of the MMA disappearing during the first final polymerization attempt?
The initiator might have been old or bad, leading to insufficient pre-polymerization.
What change was made to the pre-polymerization process after the initial failure?
Twice the amount of initiator was used.
How did the visual cues change during the pre-polymerization with increased initiator?
Small gas bubbles (nitrogen) were released, and the solution got thicker and thicker over 15 minutes, indicating that the initiator was working and polymerization was occurring.
After the second attempt at final polymerization, what major problem was encountered when trying to remove the piece from the glass?
The acrylic was stuck to the glass.
How was the transparent wood piece eventually freed from the stuck glass?
Scorelines were made in the glass, and it was carefully smashed with a hammer. A dremel was then used to cut off extra bits of plastic, and it was sanded.
What two main issues were identified from the first partially successful transparent wood piece?
The piece was still super hazy and very yellow, indicating that the wood hadn't been treated long enough (too much lignin) and the pieces were made too thick.
What changes were made to the wood preparation in the subsequent attempts to improve transparency?
Thinner pieces of balsa wood (1.5mm) were used, and they were treated until completely white, taking about seven hours.
What solvent was substituted for ethanol during the drying process in later attempts, and why?
99% isopropyl alcohol, because it was way cheaper.
What improvements were made to the glass plates used for sandwiching the wood during polymerization?
Thicker, stronger glass coasters were used, and they were sprayed with mold release to prevent the acrylic from sticking.
What was the purpose of applying mold release to the glass plates?
To prevent the acrylic from getting stuck to the glass.
What issue arose in the subsequent attempt when the wood was sandwiched between glass, despite using mold release?
The glass had somehow tipped over, and while the top glass popped off, the actual wood piece still didn't pop off nicely.
How was the problem of the glass tipping over fixed?
Spacers cut from untreated balsa were added to hold the glass plates level, and aluminum tape was used to hold everything in place.
What change was made to the mold release application after the wood still got stuck?
Four layers of mold release were applied to the glass instead of just two.
What was the main imperfection of the resulting transparent wood piece even after multiple refinements?
The top side was still a bit rough, while the bottom side (touching the bottom plate) was almost completely smooth and shiny.
What was hypothesized to fix the rough top surface of the transparent wood, and how was it attempted?
By putting some weight on it to really squish the pieces together, using a 5-pound tungsten cube.
What was the main challenge encountered when scaling up the transparent wood process?
Any gas bubbles that formed had a much harder time escaping, especially if they formed near the middle of the piece.
What was found to be a critical and difficult part of the pre-polymerized methacrylate preparation when scaling up?
Achieving an optimal thickness or viscosity, which never seemed to take the same amount of time (ranging from 15 to 40 minutes).
What change was made to the amount of initiator when preparing pre-polymerized methacrylate for the final successful large piece?
Used a lot less initiator, only 20% more than the original amount, instead of double.
What change was made to the vacuum cycles for the larger pieces during infusion, and why?
The vacuum cycles were much longer, about 45 minutes each, and the strongest possible vacuum was pulled to get rid of all acetone and unpolymerized methacrylate.
What was a side effect of the extended vacuum cycles during methacrylate infusion?
The methacrylate thickened a lot more, making it important to start with methacrylate that wasn't too thick.
What was identified as sabotaging the process of achieving a smooth top surface, and why?
Small wood spacers. Methyl methacrylate contracts by up to 21% as it polymerizes, pulling the piece away from the upper glass plate, making the added weight ineffective.
What alternative was found for balancing the glass plates on larger pieces after removing the wood spacers?
The piece of wood itself was large enough that it wasn't an issue balancing the glass plate on it, as long as it was kept more or less centered.
What heavy object was used to apply pressure during the final polymerization of the large transparent wood piece?
A 40-pound tungsten cube.
What modification was made to the oven heating process for the final large transparent wood piece?
The oven was not preheated; it heated up slowly from room temperature.
What was the final process to refine the surface of the transparent wood piece?
Wet sanding starting with 600 grit, going down to 320, then gradually moving up to 2500 grit, followed by polishing with Novus plastic polish (numbers 3 and 2).
What was the final assessment of the successful transparent wood piece?
It was way better than expected, very transparent with easily readable text, and the slight imperfections made it look more like wood than plastic, with the grain being more obvious.
What minor flaw was still noticeable in the final transparent wood piece when against white paper?
It had a slight yellow tint to it.