Transistors and Moore’s Law

Extreme Ultraviolet Lithography and the Machines That Make Advanced Chips

1. Transistors, chip performance, and Moore’s Law

A microchip is a dense system of electronic components connected by layers of wiring. At its foundation are transistors, which act as controllable switches and represent the basic on-and-off states used in digital computing.

Shrinking transistors has two major benefits:

  • Signals travel shorter distances. Electrons have less distance to move between components, which can help circuits operate faster.

  • More transistors fit in the same area. A chip with more transistors can perform more computations and support more complex functions.

For decades, improvements in manufacturing allowed transistor sizes to decrease and transistor counts to grow. The observed trend that the number of transistors on a chip roughly doubled about every two years became known as Moore’s Law. It was an empirical pattern, not a physical law, but it helped describe and drive progress in the semiconductor industry.

By around 2015, conventional manufacturing methods were approaching physical and engineering limits. Continuing to shrink chip features required a major improvement in the technology used to print circuit patterns onto silicon.


2. How a silicon wafer becomes a chip

Chip fabrication begins with extremely pure silicon and proceeds through many repeated patterning steps.

2.1 Making silicon wafers

  1. Silicon dioxide, commonly obtained from sand, is purified to produce nearly pure silicon.

  2. The silicon is melted in a furnace.

  3. A small seed crystal is lowered into the molten silicon. Silicon atoms attach to the seed in an orderly arrangement.

  4. The seed is slowly raised and rotated, producing a large, single-crystal silicon ingot.

  5. Diamond wire saws slice the ingot into thin wafers, which are then carefully polished.

The single-crystal structure provides a uniform foundation for building precise electronic devices.

2.2 Patterning a wafer

A chip is built through repeated cycles that create and shape materials on the wafer. A simplified cycle is:

  1. Coat: Apply a light-sensitive material called photoresist.

  2. Expose: Shine patterned light onto the photoresist.

  3. Develop: Use a solution to remove selected parts of the photoresist.

  4. Etch and deposit: Etch exposed regions of the underlying material, then deposit materials such as metal into the resulting structures.

  5. Remove remaining resist: Wash away photoresist that is no longer needed.

In positive photoresist, areas exposed to light become more soluble, so they can be removed during development. The remaining resist protects selected parts of the wafer during later processing.

The cycle is repeated to create the many layers in a chip. A chip can contain roughly 10 to 100 layers:

  • The lowest layer contains the transistors and is especially complex.

  • The upper layers contain metal wiring that carries signals and power between devices.

A completed wafer may contain hundreds of chips. The wafer is cut into individual pieces, which are then packaged for use in electronic products.


3. Photolithography: printing the circuit pattern

Photolithography is the process of using light to transfer a pattern onto a wafer. It is crucial because the wavelength of the light and the optical system help determine the smallest features that can be printed.

A patterned plate called a mask, or reticle, carries the design for one chip layer. Light passes through or reflects from the pattern and is directed onto the wafer, where it alters the photoresist.

3.1 Diffraction and interference

Light behaves as a wave. When it passes through narrow openings in a mask, the waves spread out. This spreading is called diffraction.

Waves from neighboring openings overlap and interfere:

  • If a peak from one wave meets a trough from another, they cancel, producing a darker region.

  • If peaks meet peaks, or troughs meet troughs, they reinforce one another, producing a brighter region.

The resulting light pattern is called a diffraction pattern. Diffraction cannot be eliminated, so lithography designers account for it and shape mask patterns to produce the desired image on the wafer.

To form a clearly resolved pattern, the optical system must capture the central, or zero-order, light and important first-order diffracted light. As printed features get smaller, the angle between these orders grows, so the optical system must capture light over a wider range of angles.

3.2 Numerical aperture and wavelength

The light-gathering ability of an optical system is described by its numerical aperture (NA). In a simplified description, NA is related to the sine of the maximum collection angle, α\alphaα:

NA=sin⁡(α)\mathrm{NA} = \sin(\alpha)NA=sin(α)

A larger NA lets the system capture more widely angled diffracted light and can help it print smaller features. However, increasing the angle has a practical limit.

The other important factor is the wavelength of the light. Shorter wavelengths can print smaller patterns using the same optical system, because the diffracted orders remain closer together.

The relationship is summarized by the Rayleigh criterion:

CD=k1λNA\mathrm{CD} = k_1 \frac{\lambda}{\mathrm{NA}}CD=k1​NAλ​

Here, CD\mathrm{CD}CD is the critical dimension, or smallest printable feature size; λ\lambdaλ is the light’s wavelength; and k1k_1k1​ represents process and design factors. Smaller wavelengths and larger numerical apertures reduce the critical dimension.

For many years, the industry used progressively shorter wavelengths. By the late 1990s, it had settled on 193-nanometer deep ultraviolet light for advanced chip production. By around 2015, further improvements using that wavelength were no longer enough to keep conventional scaling on track. A new, much shorter wavelength was needed.


4. The idea behind extreme ultraviolet lithography

In the 1980s, Japanese scientist Hiroo Kinoshita proposed using much shorter-wavelength radiation—around 10 nanometers—to print smaller features. This approach eventually became known as extreme ultraviolet lithography, or EUV lithography.

EUV offered a way to continue shrinking features, but it created several major problems:

  • EUV radiation is strongly absorbed by many materials.

  • Air absorbs it, so the optical path must be kept in a vacuum.

  • Ordinary lenses absorb EUV, so the system must use mirrors instead.

  • The mirrors must be extraordinarily smooth to prevent the light from scattering.

  • A sufficiently powerful, reliable EUV source is difficult to make.

This meant that EUV required a complete optical and manufacturing system, not simply a different light bulb.


5. Multilayer mirrors: reflecting light that ordinary optics absorb

A mirror normally reflects light at a boundary between materials. How much light is reflected depends on factors including the angle of incidence, polarization, and the materials’ refractive indices.

For EUV, a single boundary reflects too little light. Researchers therefore developed multilayer mirrors: stacks of extremely thin alternating layers designed so that small reflections from many boundaries reinforce one another.

5.1 Constructive reflection from layered materials

A thin layer of tungsten and a layer of carbon can be arranged so that:

  1. Some EUV light reflects at the first boundary.

  2. Some light passes through and travels within the layers.

  3. Reflections from different boundaries acquire carefully chosen phase differences.

  4. The reflected waves line up and interfere constructively, increasing the total reflected light.

The layer thicknesses are tuned to the light’s wavelength. Repeating the layers many times increases the total reflection. Early tungsten-carbon mirrors demonstrated the principle that x-ray-range radiation could be reflected, although their reflectivity was low.

Later research focused on material combinations with greater potential reflectivity. Molybdenum and silicon proved useful for light near 13 nanometers. Another candidate, molybdenum and beryllium, offered higher theoretical reflectivity at a somewhat shorter wavelength, but beryllium is highly toxic and difficult to handle.

5.2 The need for extreme smoothness

If a mirror’s surface roughness is large compared with the wavelength, light scatters in many directions instead of reflecting cleanly. EUV mirrors therefore need surfaces that are smooth at nearly atomic scales.

The required smoothness is so extreme that, if a mirror were enlarged to a country-sized surface, its largest bump would be only about a millimeter high. The more advanced high-NA mirrors are smoother still: if enlarged to the size of the world, their largest bump would be about the thickness of a playing card.

Making such surfaces requires carefully controlled coating processes. In sputtering, plasma or ions strike a target material, knocking atoms loose so that they travel to and deposit on the mirror. Because this process can create small irregularities, ion-beam methods are used to help atoms settle into gaps and produce flatter layers.


6. From early demonstrations to a commercial technology

The idea of EUV lithography was repeatedly doubted because it demanded capabilities that seemed unrealistic: a powerful EUV source, nearly perfect mirrors, and a vacuum optical system.

Kinoshita demonstrated early x-ray lithography by using curved multilayer mirrors to print patterns. His work showed that the approach was physically possible, but the early printed features were far larger than those eventually needed for advanced chips. Critics also questioned how such a system could be made useful for manufacturing.

Work at national laboratories added important evidence. Researchers studying x-rays produced in high-energy and fusion-related experiments developed multilayer mirrors and explored their use in lithography. Early commercial applications remained difficult, and proposals for x-ray lithography were often met with skepticism.

6.1 Shared research and public-private investment

Government-supported laboratories had accumulated expertise with materials, optics, and radiation sources. As Cold War investment slowed, governments encouraged laboratories to work with companies to turn research into commercial technologies.

This cooperation helped sustain EUV development. When government funding for the project was cut in the 1990s, major semiconductor companies—including Intel, Motorola, and AMD—invested to keep the research going.

By 2000, researchers had built an Engineering Test Stand, a functioning EUV prototype. It generated 13.4-nanometer light and used multiple mirrors to direct it from the source, through the mask, and onto the wafer. It could print features around 70 nanometers wide, showing that an EUV system could work.

However, the prototype produced only about 10 wafers per hour. Commercial chip production required a system capable of producing hundreds of wafers per hour, continuously and reliably. Demonstrating the basic physics was only the beginning; the equipment had to become a dependable factory tool.


7. Why the prototype was too slow

EUV light loses intensity every time it reflects from a mirror. A mask also has to act as a mirror, because a conventional transmissive mask would absorb the EUV light.

Even high-quality mirrors reflect only a fraction of the light that reaches them. With six mirrors and a reflective reticle, the amount of light reaching the wafer is only a small fraction of the original amount. Too little light means that wafers are exposed slowly, limiting production.

The system cannot simply remove most of its mirrors. Optical systems introduce distortions called aberrations. In a lens system, for example, rays passing through the outer part of a lens may focus differently from rays near the center. Multiple optical elements help correct such errors; mirror-based systems also need enough mirrors to control aberrations.

The challenge was therefore to increase the EUV source power while preserving the accuracy of the optical system.


8. Choosing and producing the EUV wavelength

A lithography system must use a wavelength that both the light source can produce and the mirrors can efficiently reflect. Early work considered several wavelengths. The selected commercial system used light near 13.5 nanometers because multilayer mirrors made from molybdenum and silicon could reflect it effectively.

8.1 Why synchrotrons were not suitable as factory sources

Early researchers often used particle accelerators or synchrotrons to generate EUV light. These sources could produce substantial power, but a factory could not rely on one large shared accelerator: each manufacturing tool needed its own source. A compact source integrated with each machine was necessary.

8.2 Discharge-produced plasma

One method is to heat a material into vapor and apply a strong electric field. Free electrons collide with atoms, producing ions. When the electric field is removed, electrons recombine with ions and emit photons.

This is called discharge-produced plasma. It was relatively simple and could produce some EUV power, but scaling it to the power needed for commercial manufacturing proved difficult.

8.3 Laser-produced plasma

The scalable approach became laser-produced plasma. A powerful laser strikes a target, creating an extremely hot plasma. Electrons become energetic enough to leave their atoms; when they later recombine with ions, the plasma emits light.

The Engineering Test Stand used a laser to strike xenon gas. Xenon could emit light near the desired EUV range, but much of its energy went into other wavelengths that the mirrors could not reflect efficiently. Neutral xenon atoms also absorbed some of the useful EUV light. Its conversion efficiency—the fraction of input power converted to usable EUV—was only about 0.5%.

Tin offered a better emission peak near 13.5 nanometers and substantially higher conversion efficiency. But tin introduced a serious problem: tin debris could contaminate the machine’s expensive collector mirror.


9. Tin droplets and the laser-produced plasma source

The commercial EUV source uses tiny molten tin droplets as targets. Producing and hitting them reliably is a difficult engineering task.

9.1 Producing uniform, fast-moving droplets

Pure tin is melted and pushed through a microscopic nozzle using high-pressure nitrogen. The nozzle vibrates at a selected frequency, breaking the stream into droplets.

The raw stream is irregular, but careful control of the flow and vibration causes it to form droplets that are similar in size and shape, regularly spaced, and moving at predictable speeds. Early commercial systems used about 50,000 droplets per second.

Droplets must be separated and fast enough that one plasma event does not interfere with the next. Their movement must also be controlled despite the complex flow of hydrogen inside the source.

9.2 Hitting a droplet twice

A single powerful laser pulse does not use the tin efficiently. The improved method uses two stages:

  1. A first laser pulse hits a droplet and flattens it into a pancake.

  2. A stronger main pulse hits the expanded target and turns the tin into plasma.

Flattening the droplet gives the main pulse a larger surface area to vaporize. This increases the useful EUV output without simply adding more tin debris or neutral atoms.

Later versions added another pre-pulse before the main pulse. The first pulse flattens the droplet; the second expands and lowers the density of the target; the final pulse ionizes it. This sequence improves the amount of EUV produced for a given amount of laser power.

9.3 Timing the laser and droplets

The laser must strike each moving droplet at precisely the right place and time. To track droplets, the system uses laser curtains: light scattered as a droplet crosses a curtain reveals its position and passage time. The source then uses that information to time the high-power laser pulse.

The targeting problem can be understood as trying to send an object into a small target while it is moving rapidly through turbulent conditions, and repeating the task tens of thousands of times per second. The source must do so reliably enough to support continuous manufacturing.


10. Controlling tin debris, heat, and mirror contamination

Each laser strike creates tin plasma, but some tin can travel toward the collector mirror. Because EUV mirrors depend on precisely controlled thin layers, even a very small amount of contamination can reduce their performance.

The source uses low-pressure hydrogen gas to help control tin debris:

  • Hydrogen slows and cools some tin particles.

  • Chemical reactions involving hydrogen help remove tin contamination by converting it into gaseous stannane.

  • New, cooler hydrogen is circulated through the system while hot gas and reaction products are removed.

This requires a careful balance. Too little hydrogen allows contamination to build up. Too much hydrogen absorbs EUV light and can increase heating.

Every plasma event also sends a shockwave through the hydrogen. Understanding these shockwaves helps engineers calculate the heat and gas flow inside the source. The system needs high-speed gas circulation to manage the repeated explosions while maintaining conditions that let EUV light travel through the chamber.


11. Increasing source power while maintaining optical alignment

Increasing source power is not enough by itself. More power produces more heat, which can slightly move or distort optical components. Even tiny changes can misalign the light and make successive chip layers fail to line up.

The system therefore uses sensors and control mechanisms to monitor mirror positions and angles with extraordinary precision. Engineers must divide a very small total error allowance among the many parts of the machine, including the source, optics, wafer stage, and reticle stage.

A useful measure of alignment between chip layers is overlay: how accurately one patterned layer is placed on top of another. Advanced EUV systems must keep overlay errors around one nanometer—only a few silicon atoms across.

Key source-power milestones

  • Early laser-produced plasma systems generated only a few watts of useful EUV power.

  • By 2011, the source had reached roughly 11 watts.

  • By 2013, it reached around 50 watts.

  • A major breakthrough came from flattening each droplet before the main pulse. By 2014, the source reached about 100 watts.

  • Further improvement was needed because other lithography techniques continued to advance, raising the performance threshold EUV had to meet.

  • Around 2015, the source reached the roughly 200-watt level needed for commercial viability.

A further difficulty involved the collector mirror’s protective coating, which degraded under the intense conditions inside the source. Experiments revealed that a small amount of oxygen in the vacuum environment helped keep the collector cleaner for longer. Combined with other contamination controls, this improvement made longer, more productive operating periods possible.


12. ASML and the commercialization of EUV

ASML, based in the Netherlands, became the company responsible for turning EUV from a difficult prototype into a manufacturing system. It worked closely with Zeiss, which developed the precision optics, while ASML concentrated on the overall lithography machine and the light source.

The project required a long-term commitment because many engineering problems had to be solved at once. ASML’s customers, including Intel, Samsung, and TSMC, invested in the company’s development so that it could continue working on the technology. Their support helped fund the effort even when promised performance targets were repeatedly missed.

An early EUV system was installed at a customer site in 2010. Installation was not the same as production readiness: the machine still experienced setbacks, and several years of further work were required before EUV could support advanced chip manufacturing.

The first commercial low-NA EUV machines used a numerical aperture of about 0.33 and could print features around 13 nanometers wide. Their adoption marked the transition from experimental EUV to factory use.


13. How a modern EUV lithography machine works

A commercial EUV machine is a large, integrated optical and mechanical system. Its major stages are:

  1. Laser amplification: A carbon dioxide laser passes through several amplifiers, increasing its power to tens of thousands of watts.

  2. Droplet targeting: The laser pulses are directed toward tin droplets moving through the source.

  3. EUV generation: Pre-pulses shape and expand each droplet; a main pulse creates plasma that emits EUV light.

  4. Collection and illumination: A collector mirror gathers EUV light. Additional mirrors shape and direct it toward the reticle.

  5. Pattern transfer: The reflective reticle carries the circuit design.

  6. Projection: Projection mirrors reduce the pattern and direct it onto the wafer.

  7. Wafer exposure: The EUV light changes the photoresist so that the pattern can be developed and transferred into the wafer.

Because EUV is absorbed by air and most materials, the optical path operates in a vacuum and relies on reflective optics rather than ordinary lenses.

13.1 High-NA EUV

The next generation, called high-NA EUV, increases the numerical aperture from about 0.33 to about 0.55. A larger NA allows smaller features to be resolved.

High-NA optics also use more complex pattern reduction. In the system described, the image is reduced by about eight times in one direction and four times in the other. The mirrors must be even smoother, and their positions and angles must be controlled extremely precisely.

The reticle moves rapidly while the wafer is exposed. Its acceleration can exceed 20 times the acceleration due to gravity. The machine coordinates this motion with the optical system so that patterns are printed quickly without sacrificing overlay accuracy.


14. Scale, cleanliness, and manufacturing infrastructure

An EUV machine’s scale reflects the difficulty of controlling light and mechanical motion at nanometer dimensions. Each machine depends on a vast supply network and many precisely integrated components.

The manufacturing system described includes:

  • Thousands of supplier companies.

  • Around 100,000 parts.

  • Thousands of cables and tens of thousands of bolts.

  • Several kilometers of tubing.

  • Hundreds of shipping containers’ worth of components distributed across trucks and cargo aircraft.

The machine is assembled and tested in an exceptionally clean environment. Even tiny particles can damage a wafer or disrupt a patterned feature. As a result, clean-room standards are far stricter than those in ordinary hospital operating rooms.

After construction and testing, the machine is partly disassembled for transport and then reassembled at the customer’s fabrication plant. Producing a tiny pattern therefore requires a very large machine, a controlled environment, precision optics, specialized lasers, and extensive factory infrastructure.


15. Why EUV mattered

EUV succeeded because it combined several technologies that had to work together:

  • Short-wavelength light for printing smaller features.

  • Multilayer mirrors capable of reflecting that light.

  • Atomically smooth optical surfaces.

  • A powerful tin-based plasma source.

  • Precise droplet generation and laser timing.

  • Contamination management and heat control.

  • Fast stages and nanometer-scale alignment.

  • A manufacturing process capable of operating reliably in a chip factory.

The technology’s significance lies not in any one component but in the integration of all of them. A failure in the light source, optics, alignment, or cleanliness could make the entire tool unsuitable for production.

The development also illustrates how difficult technological breakthroughs can be. EUV took decades of research, large investments, international collaboration, and repeated revisions to become commercially useful. Many individual obstacles seemed to make the entire project impossible, but progress came from solving them one at a time and combining the solutions into a working system.

Ask anything

We've read this whole study set, so questions about it get the best answers.

FlashcardsQuizFill in the blanksWritten testLessonNotesPodcastContent