Material Fatigue and Failure

Fatigue Failure in Materials

What fatigue is and why it matters

Fatigue is the progressive damage and eventual fracture of a material caused by repeated or fluctuating loads. A component can fail by fatigue even when the applied stresses remain below the material’s yield strength. Repeated loading gradually creates and extends cracks until the remaining material can no longer carry the load.

A familiar example is bending a metal wire back and forth. Each bend applies a stress cycle. Repeating the cycles eventually breaks the wire, even though no single bend may be strong enough to break it.

Fatigue is important in engineering because many components experience cyclic loading during normal service:

  • Rotating shafts bend under their own weight or other loads. As a shaft rotates, a point on its surface can alternate between tension and compression.

  • Automotive components experience repeated loading as vehicles travel over bumps and uneven road surfaces.

  • Aircraft structures undergo repeated loading during operation, making fatigue damage a critical safety concern.

Fatigue damage accumulates through repeated loading, and a component may fracture suddenly after appearing to function normally.


How fatigue damage develops

Fatigue failure commonly proceeds through three broad stages:

  1. Crack initiation: A small crack forms, often at a surface flaw, inclusion, sharp corner, or other stress concentrator.

  2. Crack growth: The crack extends gradually with repeated loading.

  3. Final fracture: Once the crack is large enough, the remaining material fails rapidly.

The early accumulation of damage can be slow and difficult to detect. The final fracture, by contrast, can be sudden and catastrophic. This is why a component designed to remain within the elastic range can still fail if its loading is cyclic.

Stress concentrations and crack initiation

Local stresses are often higher than the average stress in a component. This occurs near:

  • Surface scratches or defects

  • Material inclusions

  • Holes, notches, and keyways

  • Sharp corners or abrupt geometric changes

For example, a keyway in a shaft creates corners where stress can concentrate. A fatigue crack may begin at one of these locations and then grow with continued cycling.

Cyclic loading can cause localized plastic deformation near a flaw even when the overall component remains largely elastic. Repeated slip along crystallographic planes can produce small surface irregularities—often described as material moving in and out at the surface. These irregularities can develop into a sharp microcrack.


Appearance of fatigue fracture surfaces

A fatigue fracture surface often contains regions that reveal how the crack developed.

Crack origin and progressive growth region

The crack usually begins at an origin such as a flaw or stress concentration. As it grows, it can leave curved or roughly concentric markings resembling the layers of a shell. These larger-scale markings are often called beach marks or, in some descriptions, clamshell markings.

Beach marks indicate changes in crack growth or periods of crack arrest and renewed growth. They can often be seen without high magnification.

At smaller scales, the surface may show striations. These microscopic markings are associated with incremental crack advance during cyclic loading. When the conditions are suitable, the spacing between striations can provide an estimate of the crack’s growth per cycle. A striation does not necessarily correspond to one cycle in every material or loading condition.

Final fracture region

When the crack becomes sufficiently large, the remaining uncracked section can fail rapidly. This final region is the final fracture zone. Its appearance may be ductile or brittle, depending on the material, stress state, and conditions at the time of failure.


Fatigue crack-growth stages

Fatigue crack growth is often described in three stages.

Stage I: Growth along slip planes

After initiation, a small crack may grow along crystallographic slip planes. Its path is influenced by the local shear deformation and the material’s crystal structure. This early growth is generally slow, and the fracture surface may have few distinctive features.

Stage II: Growth across the material

As the crack grows, its direction increasingly becomes perpendicular to the maximum principal tensile stress. This stage commonly produces the characteristic fatigue fracture surface, including microscopic striations and, at larger scales, beach marks.

Fatigue cracks open and grow primarily under tensile loading. During the compressive part of a cycle, the crack tends to close, so substantial forward growth is limited.

Stage III: Rapid final fracture

As the crack length increases, the stress intensity at its tip also increases. When the crack reaches a critical condition, it can grow rapidly and cause final fracture. The final fracture may be ductile or brittle, depending on the material and loading conditions.


Cyclic loading and stress measures

In fatigue testing, a load cycle is often simplified to a regular waveform, such as a sinusoidal, square, or trapezoidal cycle. Actual service loads may be irregular and unpredictable, so fatigue properties must be established through testing and interpreted statistically.

For a cycle with maximum stress σmax⁡\sigma_{\max}σmax​ and minimum stress σmin⁡\sigma_{\min}σmin​, the commonly used measures are:

Stress range

The stress range is the difference between the maximum and minimum stresses:

Δσ=σmax⁡−σmin⁡\Delta \sigma = \sigma_{\max} - \sigma_{\min}Δσ=σmax​−σmin​

Stress amplitude

The stress amplitude is half the stress range:

σa=σmax⁡−σmin⁡2=Δσ2\sigma_a = \frac{\sigma_{\max} - \sigma_{\min}}{2} = \frac{\Delta \sigma}{2}σa​=2σmax​−σmin​​=2Δσ​

Mean stress

The mean stress is the average of the maximum and minimum stresses:

σm=σmax⁡+σmin⁡2\sigma_m = \frac{\sigma_{\max} + \sigma_{\min}}{2}σm​=2σmax​+σmin​​

A cycle may be entirely tensile, entirely compressive, or alternate between tension and compression. Since fatigue crack growth is promoted by tensile opening, test conditions influence how quickly cracks develop.

Stress ratio

The stress ratio is commonly defined as:

R=σmin⁡σmax⁡R = \frac{\sigma_{\min}}{\sigma_{\max}}R=σmax​σmin​​

The values of maximum stress, minimum stress, amplitude, mean stress, and stress ratio all influence fatigue behavior. A particular amplitude-to-mean-stress ratio may also be specified in a test, but its definition and use should be stated explicitly. Such a ratio is not useful when the mean stress is zero.


The stress–life curve

A common way to characterize fatigue behavior is the S–N curve, which relates cyclic stress to the number of cycles a specimen survives before failure:

  • SSS represents a stress measure, commonly stress amplitude or stress range.

  • NNN represents the number of cycles to failure.

An S–N curve is built by testing specimens at different stress levels and recording how many cycles each survives. At higher stress levels, specimens generally fail in fewer cycles. Reducing the cyclic stress generally increases the number of cycles to failure.

Fatigue properties vary among specimens and conditions, so fatigue testing usually requires multiple tests and statistical treatment. The results depend on factors such as mean stress, stress amplitude, material condition, environment, and test method.

Endurance limit

Some steels show an endurance limit: below a certain stress amplitude, the material can withstand a very large number of cycles without fatigue failure, under the conditions represented by the test.

Aluminum alloys generally do not show a clear endurance limit. Their fatigue life continues to increase as the stress amplitude decreases, but a sufficiently large number of cycles can still eventually cause failure. Thus, a very long fatigue life is not the same as an unlimited life.


Stress intensity and fatigue crack growth

Once a crack exists, its growth is influenced by the stress intensity factor, which describes the intensity of the stress field near the crack tip. During a cycle, the stress intensity factor varies between a maximum and a minimum value. The range is:

ΔK=Kmax⁡−Kmin⁡\Delta K = K_{\max} - K_{\min}ΔK=Kmax​−Kmin​

For many common crack geometries, the stress intensity range can be expressed in the form:

ΔK=Y Δσπa\Delta K = Y \, \Delta \sigma \sqrt{\pi a}ΔK=YΔσπa​

Here, aaa is crack length and YYY is a factor that depends on the geometry and loading arrangement. Because ΔK\Delta KΔK depends on crack length, it generally increases as the crack grows, even if the applied stress range stays constant.

Paris law

In a middle range of fatigue crack growth, the crack-growth rate is often approximated by Paris law:

dadN=C(ΔK)m\frac{da}{dN} = C(\Delta K)^mdNda​=C(ΔK)m

where:

  • aaa is crack length.

  • NNN is the number of load cycles.

  • dadN\frac{da}{dN}dNda​ is the crack extension per cycle.

  • ΔK\Delta KΔK is the stress intensity range.

  • CCC and mmm are material and test-condition constants.

Some sources use different symbols for crack length or for the constants, but the relationship has the same form. The constants depend on the material, environment, and testing conditions, and their numerical values depend on the units used.

Reported exponents are often around 333 for some steels and aluminum alloys, about 3.33.33.3 for nickel, and about 555 for titanium. These are representative values, not universal constants.

Three regions of crack-growth behavior

A typical plot of crack-growth rate against ΔK\Delta KΔK has three regions:

  1. Near-threshold region: At low ΔK\Delta KΔK, crack growth is extremely slow or may be negligible under the test conditions.

  2. Paris-law region: Over an intermediate range, crack-growth rate follows the power-law relationship above.

  3. Rapid-growth region: At high ΔK\Delta KΔK, the crack accelerates toward unstable fracture as the material’s critical fracture condition is approached.

As a crack grows, the increasing crack length tends to raise the stress intensity. A crack can therefore progress from slow growth to accelerated growth and finally to catastrophic fracture.


Factors that influence fatigue life

Surface finish

Surface defects can act as crack-initiation sites. Improving surface finish through processes such as grinding or buffing can remove or reduce small surface irregularities and thereby improve fatigue life.

Grain size

Grain boundaries can obstruct crack propagation. A smaller grain size generally creates more grain-boundary area, increasing the number of obstacles a crack must negotiate. Under suitable conditions, this can improve fatigue resistance.

Residual stress

Residual stresses are stresses that remain in a material after processing. Compressive residual stress at the surface can improve fatigue performance because it counteracts some of the applied tensile stress and helps keep surface cracks closed.

Shot peening is one method used to introduce compressive residual stress. Small steel balls are directed at the surface at high velocity, plastically deforming the near-surface region and leaving it in compression.

Environment and corrosion

Corrosion can damage a surface and create flaws that encourage crack initiation. A corrosive environment can therefore reduce fatigue life, particularly when the material is also subjected to cyclic loading.


Design and assessment implications

Fatigue design cannot rely only on keeping the maximum stress below the yield strength. Repeated stresses below yield can still cause progressive crack initiation and growth.

A reliable assessment considers:

  • The cyclic loading pattern and its maximum and minimum stresses

  • Stress amplitude, stress range, mean stress, and stress ratio

  • Geometric stress concentrations and surface condition

  • Material fatigue data and the statistical scatter in test results

  • Crack-growth behavior and the possibility of inspection or replacement

  • The effects of residual stress, grain structure, and environment

Monitoring and maintenance are important because fatigue damage may accumulate gradually but end in sudden fracture. Understanding crack-growth rates can help estimate how a flaw may develop and when a component should be inspected or replaced.

Ask anything

We've read this whole study set, so questions about it get the best answers.

FlashcardsQuizFill in the blanksWritten testLessonNotesPodcastContent