Material Fatigue and Failure

Speaker 1Speaker 2

Material Fatigue and Failure

10:13
0:00-10:13
  1. Corey

    Today we’re talking about fatigue, a way materials can fail after repeated loading. You may have seen a simple version of it: bend an aluminum wire back and forth, and eventually it breaks. The bending is the repeated load; with a large enough stress amplitude, the wire may fracture in relatively few cycles.

  2. Maria

    And the important point is that fatigue isn’t limited to a wire being deliberately bent. Many engineering parts experience repeated changes in stress during ordinary service. A rotating shaft, for example, can have tension on one side and compression on the other as it bends under its own weight. As it rotates, a point on the shaft repeatedly moves through those stress conditions.

  3. Corey

    Automobiles are another everyday example. As a vehicle travels over bumps, its components experience changing loads, which can create fatigue loading. So fatigue matters because a component can be repeatedly stressed even when no single load seems extreme.

  4. Maria

    That leads to the surprising part: a material can fail from fatigue even if its stress stays below the yield point. A design may keep service stresses far below the yield stress, with a safety margin, yet repeated loading can still accumulate damage and eventually fracture the part.

  5. Corey

    Fatigue failure often begins slowly and can end suddenly. A crack develops and grows over many cycles, but once it reaches a critical size, the remaining material can fracture catastrophically. That sudden final break is one reason fatigue is such a serious engineering problem.

  6. Maria

    Fracture surfaces can preserve clues about that history. You may see a crack origin, a region showing gradual crack growth, and a final fracture zone where the remaining material broke. A stress concentration can help explain where the crack began: for example, a shaft’s keyway can have sharp corners where stress becomes locally high.

  7. Corey

    So we can divide fatigue failure into three broad parts: crack initiation, crack growth, and final catastrophic fracture. The fracture surface may show concentric markings that look like a clamshell or shell pattern. Those visible marks help indicate where the crack started and how it spread.

  8. Maria

    There are also finer features. At a larger scale, beach marks or clamshell-like markings can record changes or pauses in crack growth. Under a microscope, much finer striations may appear. They’re associated with stepwise crack advance, and measuring the spacing between striations can help estimate how far the crack grew per cycle.

  9. Corey

    How does a fatigue crack start in the first place? A flaw, an inclusion, a design feature, or another stress concentration can raise the local stress. Repeated loading can then cause local plastic deformation even though the overall applied stress is below the yield point.

  10. Maria

    That local deformation involves slip along crystal planes, especially where shear stress is high. As the loading reverses, slip can move in and out at the surface. Repeated motion can leave a very sharp, crack-like feature, providing a starting point for a fatigue crack.

  11. Corey

    Once initiated, the crack grows in stages. In the first stage, it tends to follow a slip plane, so its path is influenced by the crystal structure. This early growth is slow, and the fracture surface may have few obvious features.

  12. Maria

    In the second stage, the crack turns to grow roughly transverse to the principal normal stress. This is where fatigue striations are often observed microscopically, while broader beach marks may be visible across the fracture surface. The crack continues to advance until it becomes large enough for rapid failure.

  13. Corey

    That final stage begins when the crack reaches a critical condition. If the stress intensity factor for the crack exceeds the material’s critical stress intensity factor, rapid fracture occurs. Whether that final fracture looks ductile or brittle depends on the material and its stress state.

  14. Maria

    The opening and closing of the crack helps explain the markings. A fatigue crack propagates mainly when it is open in tension. During compression, it tends to close; when tension returns, it can advance again. Repeated advance and closure can produce stepwise features such as striations.

  15. Corey

    To study fatigue, engineers apply repeated stress cycles. Real service loads can be irregular and unpredictable, but tests often use simplified cycles, such as sinusoidal, square, or trapezoidal waveforms. Because actual fatigue behavior varies, material properties are generally established statistically using many tests.

  16. Maria

    For a stress cycle, we define the maximum stress, sigma max, and the minimum stress, sigma min. The stress range is delta sigma, or sigma r, and equals sigma max minus sigma min. The stress amplitude is half the range: sigma a equals sigma max minus sigma min, divided by two.

  17. Corey

    The mean stress is the average of the maximum and minimum: sigma mean equals sigma max plus sigma min, divided by two. Another useful quantity is the stress ratio, R, which is sigma min divided by sigma max. The amplitude ratio can be expressed as stress amplitude divided by mean stress. These values describe the cycle used in a fatigue test.

  18. Maria

    The particular cycle matters. A cycle may include both tensile and compressive stresses, or its maximum and minimum may both be tensile. Since cracks tend to advance when open in tension, fatigue tests may use tensile conditions to encourage faster crack growth. The chosen stress range, mean stress, and stress ratio all affect fatigue behavior.

  19. Corey

    A common way to summarize test results is an S–N curve: stress, often stress amplitude or range, plotted against the number of cycles to failure. Each test tells you how many cycles a specimen survives at a chosen stress level. In general, a larger stress range means fewer cycles to failure; reducing the range usually lets the material survive more cycles.

  20. Maria

    You need many tests at different stress levels and cycle conditions to build a reliable curve. For some steels, the curve levels off at an endurance limit. Below that stress amplitude, the steel can withstand very many cycles without fatigue failure, according to this model.

  21. Corey

    That endurance limit is not a feature of every material. Aluminum, for example, does not show the same clear limit in the curve described here. Its fatigue life continues to depend on stress amplitude, so it may eventually fail after a sufficiently large number of cycles, even at lower stress levels.

  22. Maria

    For a crack that already exists, engineers also want to know how quickly it will grow. Paris law relates crack growth per cycle to the change in stress intensity factor during the cycle. In common notation, da over dN equals A times delta K raised to the power p, where a is crack length and N is the number of cycles.

  23. Corey

    Delta K is K max minus K min: the stress intensity factor at maximum stress minus the value at minimum stress. The constants A and p depend on the material, environment, and test conditions. The source gives p values of about 3 for steel and aluminum, 3.3 for nickel, and 5 for titanium.

  24. Maria

    A crack-growth-rate plot against delta K has three useful regions. At low stress intensity, growth is very slow or may be near a threshold. In the middle region, the crack-growth rate follows the Paris-law relationship. At higher values, growth accelerates until the crack reaches the critical condition and failure becomes unstable.

  25. Corey

    Even during one test, delta K can change as the crack grows, because crack size affects the stress intensity factor. That means the crack-growth rate can move from the slower region through the Paris-law region and into rapid, unstable growth.

  26. Maria

    Several practical factors affect fatigue life. Surface finish is one: scratches and small surface defects can act as stress concentrators and encourage crack initiation. Grinding or buffing to improve the finish can remove some of those defects and improve fatigue performance.

  27. Corey

    Grain size matters too. Grain boundaries can obstruct crack propagation because the direction a crack favors in one grain may not align with the next grain. Smaller grains mean more grain-boundary area, creating more obstacles to crack growth and generally improving fatigue life.

  28. Maria

    Residual stress is another factor. Compressive stress at the surface helps close cracks. When an applied tensile load acts on a surface with compressive residual stress, some of that applied tension is offset, reducing the effective tension experienced by the crack.

  29. Corey

    Shot peening is one way to introduce compressive stress at a surface. Small steel balls strike the material at high speed, leaving compressive residual stresses that can help resist fatigue crack growth.

  30. Maria

    And the environment matters. Corrosion can create flaws that act as crack-starting sites, so a corrosive environment can make fatigue more damaging. When designing or using a component under repeated loading, it’s important to consider its environment as well as its stress cycle, surface condition, grain size, and residual stresses.

  31. Corey

    So the full picture is that fatigue damage builds through repeated loading, often below the yield point. A crack initiates at a flaw or stress concentration, grows gradually with each cycle, and may ultimately trigger a sudden final fracture.

  32. Maria

    And engineers use fatigue tests, S–N curves, crack-growth measurements, and Paris law to characterize and manage that risk. Understanding where cracks start, how they grow, and what conditions speed them up helps make components safer and helps guide decisions about inspection and replacement.

Ask anything

We've read this whole study set, so questions about it get the best answers.