Material Fatigue and Failure
- 51Unfamiliar
- 0Learning
- 0Familiar
- 0Mastered
What is fatigue failure, and what kind of loading causes it?
51 questions
- 1
What is fatigue failure, and what kind of loading causes it?
Model answer
Fatigue failure is damage and eventual fracture caused by repeated cyclic loading. It can occur even when the loads are below the material’s yield point.
Explanation
Repeated loading accumulates damage over time, which can eventually produce a fracture.
- 2
How can repeatedly bending a metal wire demonstrate fatigue?
Model answer
Repeatedly bending the wire applies cyclic stresses that accumulate damage until the wire breaks. A high stress amplitude can make the fracture occur quickly.
Explanation
The repeated bending and unbending acts as a fatigue test.
- 3
Why does a rotating shaft experience cyclic tensile and compressive stresses?
Model answer
A shaft that bends under its own weight has tensile stress on one side and compressive stress on the other. As it rotates, each location alternates between tension and compression.
Explanation
Rotation repeatedly changes which side of the shaft is in tension and which is in compression.
- 4
How can road conditions expose automobile materials to fatigue loading?
Model answer
Repeated movement over bumps subjects automobile components to repeated, changing loads, creating fatigue loading.
Explanation
The loads recur as the vehicle travels, rather than being applied only once.
- 5
What kind of structural failure was identified in the damaged aircraft example, and what caused it?
Model answer
The structure failed by fatigue after experiencing repeated cyclic loading.
Explanation
Investigation traced the failure to fatigue loading of the aircraft structure.
- 6
Why can fatigue be dangerous even when a component is designed to remain below its yield stress?
Model answer
Repeated service loads can accumulate fatigue damage and cause fracture even when the stress remains below the yield stress.
Explanation
Staying within the elastic regime does not by itself prevent fatigue failure.
- 7
How does fatigue damage typically progress before failure?
Model answer
Damage accumulates gradually under repeated loading, but the component may then fracture suddenly and catastrophically.
Explanation
The slow accumulation of damage can make the final fracture appear abrupt.
- 8
What are the three broad stages of fatigue failure?
Model answer
The stages are crack initiation, crack growth, and final catastrophic fracture.
Explanation
Fatigue failure progresses from the formation of a crack to its propagation and eventual rapid fracture.
- 9
How can a flaw or design feature such as a keyhole contribute to fatigue crack initiation?
Model answer
A flaw or sharp corner creates a stress concentration, raising the local stress enough to promote deformation and crack initiation.
Explanation
In a shaft, sharp corners around a keyhole can act as crack-initiation sites.
- 10
What fracture-surface features can indicate fatigue, and where does the final fracture occur?
Model answer
Fatigue surfaces can show markings that spread from a crack origin; the remaining section eventually fails in a final fracture zone.
Explanation
The markings record crack development, while the final zone forms when the remaining material fractures.
- 11
What do concentric clamshell markings on a fatigue fracture surface indicate?
Model answer
They indicate progressive crack propagation outward from an initiation site, often associated with a flaw or stress concentration.
Explanation
The concentric markings trace the advancing crack front.
- 12
How do clamshell markings and striations differ in scale and visibility?
Model answer
Clamshell markings can be visible in an ordinary photograph, whereas striations are finer features observed microscopically.
Explanation
Striations occur within the broader clamshell-marked region.
- 13
What do fatigue striations represent?
Model answer
They record stepwise crack advance, with each striation corresponding to crack growth during a loading cycle.
Explanation
Measuring the spacing between striations can indicate how far the crack advanced per cycle.
- 14
Why does a fatigue crack generally advance during the tensile part of a cycle rather than the compressive part?
Model answer
Tensile stress opens the crack and allows it to advance, whereas compressive stress tends to close it.
Explanation
Repeated opening and closing produces incremental crack growth.
- 15
How can the spacing between striations be used to estimate fatigue crack growth?
Model answer
The distance between adjacent striations can be used to estimate the crack extension during one loading cycle.
Explanation
Each striation marks a step of cyclic crack advance.
- 16
What happens to a fatigue crack when its stress intensity factor exceeds the material’s critical stress intensity factor?
Model answer
The crack becomes unstable and rapid fracture occurs.
Explanation
Once the critical condition is reached, the remaining crack growth is catastrophic.
- 17
What determines whether the final rapid fracture is ductile or brittle?
Model answer
The fracture mode depends on the state of stress and the condition of the material.
Explanation
Both ductile and brittle final fracture are possible once the crack meets the rapid-propagation criterion.
- 18
How does local plastic deformation help initiate a fatigue crack?
Model answer
Stress concentrations near flaws can cause localized plastic deformation during cycling, allowing a crack to form.
Explanation
The local stress may be high enough to deform material even when the overall applied stress is lower.
- 19
What role does cyclic slip along crystal planes play in fatigue crack initiation?
Model answer
Repeated slip moves crystal planes back and forth, causing localized surface displacement that can develop into a sharp crack.
Explanation
The repeated in-and-out motion associated with slip creates a crack-like discontinuity.
- 20
Describe the three stages of fatigue crack growth.
Model answer
In stage one, the crack grows along a slip plane; in stage two, it grows transverse to the principal normal stress; in stage three, it grows unstably toward final fracture.
Explanation
The stages progress from localized crystallographic growth to stress-directed propagation and then catastrophic growth.
- 21
What are the typical characteristics of stage-one fatigue crack growth?
Model answer
The crack follows a slip plane, often producing a relatively featureless, cleavage-like surface, and its growth rate is slow.
Explanation
This early growth occurs along crystallographic planes within the material.
- 22
In what direction does a stage-two fatigue crack propagate relative to the principal normal stress?
Model answer
It propagates transverse, or approximately perpendicular, to the principal normal stress.
Explanation
For example, a crack grows at about a right angle to the applied stress direction.
- 23
What surface feature is characteristic of stage-two fatigue crack growth?
Model answer
Stage two is characterized by fatigue striations on the fracture surface.
Explanation
These microscopic features record incremental crack advance during cyclic loading.
- 24
How does stage-three fatigue crack growth end?
Model answer
When the crack reaches the critical stress-intensity condition, it undergoes accelerated, unstable growth and causes catastrophic fracture.
Explanation
The final stage is rapid compared with the earlier progressive crack growth.
- 25
Why is fatigue analysis often treated statistically?
Model answer
Service stress cycles can be complex and unpredictable, and fatigue properties are determined from many tests rather than a single test.
Explanation
A range of specimens and loading conditions may be needed to characterize fatigue behavior.
- 26
What idealized loading patterns can be used in fatigue tests, and how may service loading differ?
Model answer
Tests commonly use sinusoidal, square-wave, or trapezoidal cycles, while real service loading may be random and include sudden spikes.
Explanation
Simple cycles are practical for testing, even though actual loads can be more irregular.
- 27
Define the stress range for a cyclic stress with maximum stress [0m and minimum stress [0m.
Model answer
The stress range is [0m.
Explanation
It is the difference between the maximum and minimum stresses in a cycle.
- 28
How is stress amplitude calculated from the maximum and minimum stresses?
Model answer
Stress amplitude is [0m.
Explanation
It is half the stress range.
- 29
How is mean stress calculated for a cyclic stress?
Model answer
Mean stress is [0m.
Explanation
It is the average of the maximum and minimum stresses.
- 30
How is the stress ratio defined?
Model answer
The stress ratio is the minimum stress divided by the maximum stress: R = rac{[0m}{[0m}.
Explanation
It describes the relationship between the two extreme stresses in a cycle.
- 31
How is the amplitude ratio defined in the described cyclic-loading analysis?
Model answer
It is the stress amplitude divided by the mean stress.
Explanation
The amplitude ratio is one of the parameters used to describe a stress cycle.
- 32
Why are fatigue tests sometimes run with both maximum and minimum stresses in tension?
Model answer
Tensile stress opens and propagates cracks, so keeping both stress extrema tensile can accelerate testing.
Explanation
Compressive portions of a cycle tend to close cracks rather than advance them.
- 33
What does an S–N curve relate, and how is it used?
Model answer
An S–N curve relates stress level to the number of cycles a specimen survives before failure.
Explanation
It is an empirical way to quantify fatigue behavior across different stress levels.
- 34
According to the described S–N testing approach, what stress quantity is plotted against the number of cycles?
Model answer
The stress range, [0m, is plotted against the number of cycles to failure.
Explanation
Tests at different stress ranges show how long specimens survive under each condition.
- 35
How does increasing stress range generally affect the number of cycles a material survives?
Model answer
A higher stress range generally reduces the number of cycles to failure; reducing the range generally increases fatigue life.
Explanation
S–N testing compares survival across different stress levels.
- 36
What is an endurance limit?
Model answer
It is a stress-amplitude limit below which failure will not occur, regardless of the number of cycles.
Explanation
The material’s S–N response becomes independent of cycle count below this limit.
- 37
How does the described endurance-limit behavior differ between carbon steel and aluminum?
Model answer
Carbon steel has an endurance limit, while aluminum does not; aluminum continues to show decreasing fatigue life as stress amplitude is reduced.
Explanation
Without an endurance limit, aluminum can eventually fail even after a very large number of cycles.
- 38
Why do engineers need many tests to construct a reliable fatigue-life curve?
Model answer
Fatigue behavior is statistical, so many tests at different mean stresses or stress amplitudes are needed to characterize it.
Explanation
A single test cannot establish fatigue performance across the range of possible loading conditions.
- 39
What does Paris law describe?
Model answer
Paris law relates fatigue crack growth rate per cycle to the cyclic change in stress intensity factor.
Explanation
It helps estimate how quickly a crack grows as loading cycles accumulate.
- 40
Write Paris law for crack extension per cycle and identify its parameters.
Model answer
Paris law is rac{dc}{dN} = A([0m)^p, where rac{dc}{dN} is crack growth per cycle, [0m is the stress-intensity-factor range, and A and p are constants.
Explanation
The constants depend on the material, environment, and test conditions.
- 41
How is the cyclic stress-intensity-factor range defined?
Model answer
It is [0m, where Kextmax and Kextmin correspond to the maximum and minimum stresses in the cycle.
Explanation
The range measures the change in stress intensity over a loading cycle.
- 42
What factors affect the constants in Paris law?
Model answer
The constants depend on the material, the environment, and the test conditions.
Explanation
They are not universal values that apply identically to every fatigue-growth situation.
- 43
What Paris-law exponent values are given for steel, aluminum, nickel, and titanium?
Model answer
The exponents are 3 for steel, 3 for aluminum, 3.3 for nickel, and 5 for titanium.
Explanation
These are the material-specific exponent values stated for the examples.
- 44
What are the three regions of fatigue crack growth behavior as stress-intensity range increases?
Model answer
The regions are an initial crack-growth region, a middle region described by Paris law, and a final accelerated, unstable-growth region.
Explanation
The final region leads to catastrophic failure.
- 45
Why does stress intensity change as a fatigue crack grows during a test?
Model answer
Stress intensity depends on crack size, so it changes as the crack length increases during cycling.
Explanation
Consequently, a single test can pass through different crack-growth regions over time.
- 46
How can crack-growth measurements help determine when a component should be replaced?
Model answer
Estimating crack growth per cycle helps predict how the crack will develop and when replacement may be needed.
Explanation
Paris law connects cyclic loading to crack extension over time.
- 47
How does improved surface finish affect fatigue life, and why?
Model answer
A smoother surface can improve fatigue life by removing small surface defects that could concentrate stress and initiate cracks.
Explanation
Grinding and buffing are examples of methods used to improve surface finish.
- 48
Why can reducing grain size improve fatigue life?
Model answer
Smaller grains increase grain-boundary area, and grain boundaries impede crack propagation.
Explanation
A crack may have to change direction as it encounters differently oriented grains.
- 49
How do compressive residual stresses at a surface improve fatigue resistance?
Model answer
They help close cracks and counteract part of an applied tensile stress, reducing the tensile stress experienced by the material.
Explanation
Crack closure makes further tensile-driven propagation more difficult.
- 50
What is shot peening, and how can it improve fatigue life?
Model answer
Shot peening strikes a material’s surface with small steel balls at high velocity, inducing compressive stresses that help close cracks.
Explanation
The resulting surface compression can make fatigue crack growth less likely.
- 51
How can a corrosive environment promote fatigue cracking?
Model answer
Corrosion can act like a flaw in the material and provide a site for crack initiation.
Explanation
Corrosion should be avoided in components exposed to cyclic fatigue loading.

Ask anything
We've read this whole study set, so questions about it get the best answers.